there is a way... via wet chemistry... use Gallium Chloride and Lithium Nitride with some small amount of amine then add heat check a phase diagram to see how high you have to go , but i believe 290 C is good, however this is a recipe for nanocrystalline Ga with wurtzite structure... and should...