Recent content by bamek
-
B
Regaining surface finishing after hardening stainless steel
Hi! We are going to machine some stainless steel parts that will require hardening afterwards. The parts are going to be hardened in an oven at 600 degrees celsius for 4 hours and then air cooled. This procedure is given in the suppliers data sheet. Because I'm new in the game of...- bamek
- Thread
- Stainless steel Steel Surface
- Replies: 2
- Forum: Materials and Chemical Engineering
-
B
Measuring eccentricity of the ends of a shaft
Hi! My name is Daniel and I'm new to this forum. I work as a mechanical engineer at a machining workshop in Norway. We are currently producing some steel shafts that require a high level of accuracy. The shafts are about 1500mm long, and has a diameter of 40mm h6 (+0,000mm, -0,011mm) all...- bamek
- Thread
- Eccentricity Measuring Shaft
- Replies: 2
- Forum: Mechanical Engineering