Hello,

I was in the processing of depositing BST thin films on Platinized Silicon substrate from solution using spin casting. Six layers were deposited. Each deposition was followed by 400 celsius for seven minutes and 700 celsius for three minutes. The final film was annealed for an hour at 700 celsius. The grain size seems to be in the range of 40 - 60 nm.
When doing the cross section SEM i find that there is a weird looking highly damaged layer at the bottom of the film that is around 8 um thick. The film itself is around 500 nm thick.
Does anyone have any idea what this layer is? Have you encountered it before?
The film has lower capacitance than expected, I suspect that this might be a reason why.
 
Attachments
  • Cross-sectional SEM image at 101x magnification showing a thin film layer on a substrate, with a rough, porous band along the film and a smooth substrate below; scale bar reads 10 µm, cursor height 8.888 µm.
    062312-bst-cs-10.jpg
    25.2 KB · Views: 540
  • Cross-sectional SEM micrograph of a thin film on a substrate, showing a granular, irregular layer with visible voids and cracks; scale bar 1 μm, magnification 857X.
    062312-bst-cs-7.jpg
    52.7 KB · Views: 557
Sorry... I have absolutely no knowledge of the subject. All that I can think of is oxidation of the platinum in the substrate, but I assume that you have measures in place to prevent that.