Maintaining -320°F Liquid Nitrogen for Injection Molding

AI Thread Summary
Maintaining -320°F liquid nitrogen (LN2) in a closed-loop system for injection molding poses challenges due to the narrow temperature range in which LN2 remains liquid. As LN2 absorbs heat from hot spots in the mold, it will begin to boil at -319°F, necessitating careful management of pressure to avoid explosions. Suggestions include retooling the mold with integrated cooling passages or using chilled water systems to enhance cooling efficiency. Implementing a quick shot of LN2 before plastic injection may also help in managing mold temperatures effectively. Overall, precise control and monitoring of the LN2 system are crucial for successful operation.
Diamond Dave
Messages
13
Reaction score
1
I have a plastic injection mold, the part I am running has hot spots in the part when it is being shot in the mold.
Would like to try to incorporate a closed loop plumbing system to carry liquid nitrogen past the back side of the cavity in hopes to pull the trapped heat from the hot spot area. Injected under pressure for 20 seconds. Then deplete the liquid nitrogen from the line and return it to it's holding tank. Do not want to contaminate water cooling lines, plastic material or the air quality. That is my reason for the closed system.
Now the question I have is: What do I need to maintain the −320 °F of liquid nitrogen in the holding tank?
I'm pretty sure the ambient heat when it pass through the mold will sooner or later cause the liquid nitrogen in the holding talk to boil when it reaches room temperature.
I would appreciate any input that could steer me in the right direction of maintaining -320°F
 
Engineering news on Phys.org
Diamond Dave said:
I have a plastic injection mold, the part I am running has hot spots in the part when it is being shot in the mold.
Would like to try to incorporate a closed loop plumbing system to carry liquid nitrogen past the back side of the cavity in hopes to pull the trapped heat from the hot spot area. Injected under pressure for 20 seconds. Then deplete the liquid nitrogen from the line and return it to it's holding tank. Do not want to contaminate water cooling lines, plastic material or the air quality. That is my reason for the closed system.
Now the question I have is: What do I need to maintain the −320 °F of liquid nitrogen in the holding tank?
I'm pretty sure the ambient heat when it pass through the mold will sooner or later cause the liquid nitrogen in the holding talk to boil when it reaches room temperature.
I would appreciate any input that could steer me in the right direction of maintaining -320°F
The LN2 is going to boil long before it reaches room temperature. It's going to be boiling once it reaches -319° F. In order to cool any hot spots on your mold, the LN2 must absorb some heat, and that's going to raise its temperature immediately. LN2 can remain liquid only between -346° F and -320° F, a rather narrow temperature range.

https://en.wikipedia.org/wiki/Nitrogen
 
The pressure build up will explode in a closed system. I know it's expensive, but your best bet is to retool the mold with cooling passages. Are you using chilled water in your cooling system? You can always insert a chiller in line.
 
SteamKing said:
The LN2 is going to boil long before it reaches room temperature. It's going to be boiling once it reaches -319° F. In order to cool any hot spots on your mold, the LN2 must absorb some heat, and that's going to raise its temperature immediately. LN2 can remain liquid only between -346° F and -320° F, a rather narrow temperature range.

https://en.wikipedia.org/wiki/Nitrogen
So instead of the LN2 being in the line behind the mold for 20 sec. after the material is packed. Do you think it would serve a better service
to give a quick shot before the plastic is packed. Chilling the cavity before the hot plastic reaches the area would have the same effect.
Kevin McHugh said:
The pressure build up will explode in a closed system. I know it's expensive, but your best bet is to retool the mold with cooling passages. Are you using chilled water in your cooling system? You can always insert a chiller in line.
Kevin McHugh said:
The pressure build up will explode in a closed system. I know it's expensive, but your best bet is to retool the mold with cooling passages. Are you using chilled water in your cooling system? You can always insert a chiller in line.
The tool I made is with cooling lines and the water going into the mold is coming from a chiller. What I have when I say closed loop is a hose used only for LN2 it would be on demand usage the pressure pump maintains the low line pressure. On/off valve going to intake port (copper tube) on mold. The ports are directed at and close to hot spots. Without knowing what cycle time for LN2 would be needed I would want a return line to the tank. Once it is dialed in and working It may not need a return line. It may only need an exhaust tube. LN2 has been used in molds for years but delivered a different way.
 
Back