Aluminum and copper -- Galvanic corrosion

Click For Summary

Discussion Overview

The discussion revolves around galvanic corrosion occurring between copper and aluminum when connected through a copper wire, exploring the implications for water pipes and the corrosion processes involved. Participants examine the conditions under which corrosion occurs, the roles of different metals in such connections, and the potential for protective measures.

Discussion Character

  • Debate/contested
  • Technical explanation
  • Conceptual clarification

Main Points Raised

  • Some participants suggest that copper to aluminum connections should be avoided due to the risk of corrosion, with copper corroding aluminum at the joint.
  • Others propose that treating the aluminum and copper wire as consumables could protect the copper pipe from corrosion, potentially making the aluminum a sacrificial anode.
  • There is a question about whether connecting copper wire to a less reactive metal would affect the corrosion of the wire or the pipe.
  • Some participants note that corrosion tends to be localized at the connection point rather than affecting the entire copper or aluminum structure.
  • Concerns are raised about the implications of connecting copper to galvanized steel, with some arguing that this can lead to accelerated corrosion of the steel due to galvanic action.
  • Experiences are shared regarding the failure of aluminum and copper connections, emphasizing the importance of using appropriate materials to prevent corrosion.
  • Some participants mention that using non-contact connectors can mitigate corrosion issues when connecting dissimilar metals.

Areas of Agreement / Disagreement

Participants do not reach a consensus on the best practices for connecting copper and aluminum, with multiple competing views on the implications of such connections and the effectiveness of various protective measures.

Contextual Notes

Participants express uncertainty regarding the specific conditions under which corrosion occurs, the effectiveness of sacrificial anodes, and the long-term stability of different metal connections. The discussion highlights the complexity of galvanic corrosion and the need for careful consideration of material choices.

Who May Find This Useful

This discussion may be of interest to individuals involved in plumbing, electrical work, materials science, or those seeking to understand the implications of using dissimilar metals in construction and maintenance.

Curiousphy
Messages
41
Reaction score
4
If a copper water pipe is connected to a piece of aluminum through a copper wire, where will the galvanic corrosion take place? On the wire to aluminum joint eating away at the aluminum, or will the whole water pipe suffer? (does copper corrode aluminum, or vice versa, or each other?) thanks
 
Engineering news on Phys.org
Curiousphy said:
If a copper water pipe is connected to a piece of aluminum through a copper wire, where will the galvanic corrosion take place? On the wire to aluminum joint eating away at the aluminum, or will the whole water pipe suffer? (does copper corrode aluminum, or vice versa, or each other?) thanks
Well I am not a materials expert by any means, but my years of experience tell me that
1. Copper to aluminum connections should be avoided;
2. It is the copper that corrodes the aluminum, and in the process, both the clamp and wires corrode at the connection;
3. When copper to aluminum wire connections are unavoidable, use as large a mass as possible of an aluminum bolted clamp; and
4. Install the aluminum above the copper, to prevent the copper ‘salts’ from ‘dripping’ onto the aluminum.
 
If I treat the aluminum piece and the copper wire as consumable and easily replaceable, is the copper pipe itself totally safe from corrosion through this connection? actually, would this give the copper pipe some protection and effectively make the aluminum piece a sacrificial anode?

What if the copper wire was connected to a metal that was less reactive than copper, would it corrode the wire at the connection or corrode the pipe as well? would the copper wire provide a corrosion buffer for the pipe?
 
Last edited:
Curiousphy said:
If I treat the aluminum piece and the copper wire as consumable and easily replaceable, is the copper pipe itself totally safe from corrosion through this connection? actually, would this give the copper pipe some protection and effectively make the aluminum piece a sacrificial anode?

What if the copper wire was connected to a metal that was less reactive than copper, would it corrode the wire at the connection or corrode the pipe as well? would the copper wire provide a corrosion buffer for the pipe?
Why do you not keep everything copper? Once you introduce aluminium it will create problems however you do it.
 
  • Like
Likes   Reactions: c lemmond and Asymptotic
Bulk aluminium is only stable due to the superficial oxide layer. If this is breached, the metal can corrode rapidly.

Similarly, I've known a copper hot-water tank fail because, the plumber discovered, it was resting directly on a flush floorboard nail...

Examples of rapid aluminium corrosion:
IIRC, Mercury thermometers etc are not allowed on aircraft lest break or spill attacks the structure.

'Waterglass' for sealing eggs is seriously alkaline. It ruined an aluminium pan used in error, tainted that batch of eggs. Although the 'waterglass' was labelled correctly, our complaints department sent the victim a very nice set of steel pans as 'goodwill'.

Our lab had a few aluminium weighing scoops as their 'tare' was significantly less than s/steel. I happened to find one that had sprouted a 'feather' of oxide, like a 'crystal garden', but in air. It continued growing as I watched, several mm/min. Ooh, pretty ! Sadly, I never learned what had set it off, and my few experiments failed to reproduce the effect. But we did replace those few Al scoops...
 
Curiousphy said:
If I treat the aluminum piece and the copper wire as consumable and easily replaceable, is the copper pipe itself totally safe from corrosion through this connection? actually, would this give the copper pipe some protection and effectively make the aluminum piece a sacrificial anode?

What if the copper wire was connected to a metal that was less reactive than copper, would it corrode the wire at the connection or corrode the pipe as well? would the copper wire provide a corrosion buffer for the pipe?
The aluminum becomes the anode, but in the failed corroded copper-aluminum cable connections I have seen, the corrosive failure has been limited to the immediate area at the connection. The rest of the aluminum wire and copper wire beyond the joint has undergone just the normal weathering process in forming the copper (green) and aluminum (darkened gray) oxides.
Best to use copper to copper connections, although copper to steel or copper to bronze connections are fine.
 
PhanthomJay said:
The aluminum becomes the anode, but in the failed corroded copper-aluminum cable connections I have seen, the corrosive failure has been limited to the immediate area at the connection.

Thank you, that's good to know. I know you can connect two dissimilar metals via non-contact connectors, but it's also good to know that you can use wires as corrosion buffer.
 
Last edited:
tech99 said:
Why do you not keep everything copper? Once you introduce aluminium it will create problems however you do it.

I just wanted to understand the corrosion process better. I already knew what would happen if everything was copper :)
 
  • Like
Likes   Reactions: c lemmond
@Nik_2213 Interesting story :) reminds me of youtube
 
  • Like
Likes   Reactions: Nik_2213
  • #10
PhanthomJay said:
although copper to steel or copper to bronze connections are fine.
Copper pipe connected to Galvanized pipe results in removal of the Zinc galvanize and continued corrosion of the steel pipe. Connecting them with a wire does not help; if anything it would make things worse. The Copper and Zinc, or Steel, act as a battery with the water being the electrolyte. When the are in electrical contact the battery is short circuited and starts dissolving the electrode. Same as what happens when a Carbon-Zinc flashlight battery is used, the Zinc case dissolves and it starts leaking

I lived with that for a while where the water heater was connected to the cold water pipe with Copper flex tubing (it should have been Brass or maybe Bronze rather than Copper). The result was we could not drink the tap water and the flow rate was reduced. The Iron content was so high that we got stomach aches from it! Just like if you take Iron supplement pills on an empty stomach. Ouch! (Tasted bad too.)
 
  • Like
Likes   Reactions: Curiousphy and Nik_2213
  • #11
Tom.G said:
Copper pipe connected to Galvanized pipe results in removal of the Zinc galvanize and continued corrosion of the steel pipe. Connecting them with a wire does not help; if anything it would make things worse. The Copper and Zinc, or Steel, act as a battery with the water being the electrolyte. When the are in electrical contact the battery is short circuited and starts dissolving the electrode. Same as what happens when a Carbon-Zinc flashlight battery is used, the Zinc case dissolves and it starts leaking

I lived with that for a while where the water heater was connected to the cold water pipe with Copper flex tubing (it should have been Brass or maybe Bronze rather than Copper). The result was we could not drink the tap water and the flow rate was reduced. The Iron content was so high that we got stomach aches from it! Just like if you take Iron supplement pills on an empty stomach. Ouch! (Tasted bad too.)
That is interesting. The connections I am familiar with involve stranded copper about one-half inch diameter (1.5 cm) cable in contact with a galvanized steel clamp. The clamp is much more massive than the wire, and I am unaware of any problems. I've seen several such connections about 100 years old. The clamps are heavily corroded from decades of exposure to weather, and not from the copper wire within. I still specify bronze or steel clamps when in contact with aluminum (can't afford copper clamps!).
 
  • Like
Likes   Reactions: Curiousphy
  • #12
PhanthomJay said:
That is interesting. The connections I am familiar with involve stranded copper about one-half inch diameter (1.5 cm) cable in contact with a galvanized steel clamp. The clamp is much more massive than the wire, and I am unaware of any problems. I've seen several such connections about 100 years old. The clamps are heavily corroded from decades of exposure to weather, and not from the copper wire within. I still specify bronze or steel clamps when in contact with aluminum (can't afford copper clamps!).
Different situation. I was referring to connections that were all bare metal immersed in an electrolyte such as water. I agree, exposure to weather is not usually a problem.

The OP was a bit unclear about his exact situation, so I responded to one possibile condition... and as a point of information to others.

Cheers,
Tom
 
  • Like
Likes   Reactions: Curiousphy and PhanthomJay
  • #13
Dumb question: if a copper wire bolted to aluminum wire causes corrosion, why doesn't the 90copper/10aluminum version of bronze do the same thing and corrode?

I just started looking into casting bronze (ive done some aluminum before) and it sounded like copper/aluminum is stonger/better than copper/tin. No one mentioned corrosion.
 
  • #14
Good question. I didn’t say that correctly. When connecting copper to copper , use a copper or steel or bronze clamp. When connecting aluminum to aluminum, use an aluminum or steel clamp. Now when connecting copper to aluminum, this is bad and should be avoided, but if unavoidable, use a steel or aluminum clamp where if aluminum clamp, it must be of large mass with respect to the size of the copper, and the copper should be on the bottom side so that it’s salts do not ‘drip’ onto the aluminum. This is all with air as the surrounding medium.
 
  • #15
I'd inadvertently created this Al to Cu corrosion engine, Cu ground strap connected to Al heatsink, after few weeks the ground connection would go higher resistance and subsequently melty melty.

Tinning the copper with solder before assy prevented the effect, or at least slowed it to the point it was no longer noticeable, it was a prototype, that joint was changed for for production intent lol.
 
  • #16
A number of years ago, I worked for a pulp mill. After the wood chips were cooked and pulped, the pulp, at 3% consistency, had to be separated from impurities.

This was accomplished by pumping the stock (under pressure) through cyclonic centi-cleaners attached to a stainless steel header with nylon hoses. The hoses connected to the header with standard garden hose fittings. Since SS fittings were expensive, brass connectors were often subbed in.

The punchline, after all this preamble: The process engineers decided the pulp had to be acidulated, so sulfuric acid was added upstream of the cleaners. It took about 2 days before the brass corroded enough to fail and they all blew out, spraying pulp all over. It was 3 feet deep on the floor and the mill had to shut down for 3 days for repairs.

All because nobody knew that two dissimilar metals in an acid bath would corrode.
 
  • Like
Likes   Reactions: krater, Tom.G and PhanthomJay
  • #17
Curiousphy said:
@Nik_2213 Interesting story :) reminds me of youtube
Yes, serendipitously, I came across that video just this week...


Difference, my experience lacked liquid mercury. Was it a mercury salt which deliquesced ? Or a copper salt, which had reduced to copper at a so-slightly damp scratch ? Having used 'activated zinc' in Uni organic syntheses, 'tis an enduring puzzle...
 

Similar threads

  • · Replies 9 ·
Replies
9
Views
4K
  • · Replies 9 ·
Replies
9
Views
1K
  • · Replies 8 ·
Replies
8
Views
3K
  • · Replies 9 ·
Replies
9
Views
4K
  • · Replies 16 ·
Replies
16
Views
5K
  • · Replies 1 ·
Replies
1
Views
4K
Replies
2
Views
2K
  • · Replies 6 ·
Replies
6
Views
2K
  • · Replies 2 ·
Replies
2
Views
3K
Replies
21
Views
5K