Creating Superalloys: How is Cobalt-Based Alloy Produced?

  • Thread starter Thread starter ry2ncz
  • Start date Start date
Click For Summary
SUMMARY

Cobalt-based superalloys are produced through processes such as air melting and vacuum melting, as utilized by Cannon Muskegon (The C-M Group). The production involves careful consideration of the melting points of various elements, as some may boil off during the melting process. Key references include ASM's specialty handbooks on Superalloys and Nickel/Cobalt alloys, which provide detailed processing information. Understanding these methods is crucial for optimizing the properties of cobalt alloys.

PREREQUISITES
  • Knowledge of cobalt alloy composition and properties
  • Familiarity with air melting and vacuum melting techniques
  • Understanding of melting point variations among alloying elements
  • Access to ASM specialty handbooks on Superalloys and Nickel/Cobalt alloys
NEXT STEPS
  • Research the air melting process for cobalt alloys at Cannon Muskegon
  • Explore vacuum melting techniques for improved alloy properties
  • Study the ASM specialty handbook on Nickel/Cobalt alloys for processing insights
  • Investigate the effects of different alloying elements on melting points and properties
USEFUL FOR

Materials scientists, metallurgists, and engineers involved in the production and optimization of cobalt-based superalloys.

ry2ncz
Messages
15
Reaction score
0
How are superalloys produced... I'm dealing with cobalt based alloyWhat are the process taken to produce superalloys because they could go up to 9 or 10 elements together?Cobalt is mixed with other elements for better properties but during the process of mixing some elements tend to have lower melting point... And since that is the case by the time the furnaces reaches it's melting point other elements might have just boil off...
 
Engineering news on Phys.org
Cannon Muskegon (The C-M Group. Specialty Material and Alloys Group.) does air melting and vacuum melting of cobalt alloys.

http://www.c-mgroup.com/airmelt_index/cobalt_base.htm
http://www.c-mgroup.com/vacuum_melt_index/cobalt_base.htm

ASM has specialty handbooks on Superalloys and Nickel/Cobalt alloys.

Nickel, Cobalt, and Their Alloys

Processing is covered in the texts.
 
Last edited by a moderator:
Thx for the info man I'll look into it
 

Similar threads

  • · Replies 6 ·
Replies
6
Views
4K
  • · Replies 1 ·
Replies
1
Views
6K
Replies
12
Views
6K
  • · Replies 17 ·
Replies
17
Views
27K
Replies
9
Views
3K
  • · Replies 9 ·
Replies
9
Views
2K
Replies
1
Views
5K
  • · Replies 4 ·
Replies
4
Views
1K
  • · Replies 5 ·
Replies
5
Views
3K
  • · Replies 8 ·
Replies
8
Views
4K