- #1
- 5,117
- 20
I have a question: it is generally stated that 100 micrometers is the acceptable limit on the thickness of the oxidation layer on Zircaloy4 fuel rods. But I'm at loss as what is the reason for this limit ? Is it structural integrity ? Thermal resistance ? Mechanical tolerance ?