The discussion focuses on the yield and tensile strength of Q390C high tensile steel at elevated temperatures. It is noted that most steel types generally experience a decrease in yield and tensile strength as temperature increases, with estimates suggesting a yield point retention of about 92-95% of room temperature values. The yield strength for Q390C varies from 330 MPa to 390 MPa at zero degrees Celsius, with thicker plates having the lowest minimum yield. Chemical composition details are provided, indicating specific limits for various elements. Overall, the information suggests that the yield and tensile strengths at 80 degrees Celsius are likely to be lower than the specified values at zero degrees.