Softening 8mm Allen Key - Temperature & Annealing Process

  • Thread starter Thread starter Shedfull
  • Start date Start date
AI Thread Summary
To soften an 8mm Allen key for machining, heating it above the transformation temperature of approximately 920°C and then allowing it to cool slowly is recommended. An electric muffle furnace capable of reaching 1200°C can be used for this process. The entire wrench will be annealed, which may affect its hardness. Conducting a spark test can help determine the carbon content, providing a basis for the required temperature and soaking time, typically around one hour per inch. This approach is beneficial for future reference in similar projects.
Shedfull
Messages
2
Reaction score
0
Hi, would anyone know the temperature required to soften an 8mm allen key?

I want to machine the end and thread it, from what I can gather, I need to heat it, then let it slowly cool.

I have access to an electric muffle furnace, goes to 1200°C

I know I could use hex stock, but the allen key is just the right size.:smile:


Lee.
 
Engineering news on Phys.org
I'd have to pull out my tool steels reference at work tomorrow morning. You would most likely be fine getting above the transformation temperature (920C IIRC) and furnace cooling after that. The only drawback to this is that the entire wrench is going to be annealed.

Are you stuck on doing the machining yourself? We thread hardened shafts and tools all the time. It's not difficult if you have the right tools. Do you know if there is a thread grinding shop anywhere near you? They could do it and probably would not cost you too terribly much. Just a thought.
 
stuck on the machining

Hi, I'm machining the parts myself, with no budget, but lots of ideas &
theories.

I did a bit of googling and came up with a rough solution.

here goes,

If I do a spark test on the allen key, I should get an idea of the carbon content.

Knowing the carbon content gives me a starting point for the temp.

All I have to do then is find/work out the time the part should be soaked for
(1 hr/inch?)

Am I on the right track? if so this would be good for future ref.

Lee.
 
Yes. You're on the right track. Really, a small part like an allen wrench would be completely annealed in an hour. As far as the temp, I'll have to look that one up.
 
How did you find PF?: Via Google search Hi, I have a vessel I 3D printed to investigate single bubble rise. The vessel has a 4 mm gap separated by acrylic panels. This is essentially my viewing chamber where I can record the bubble motion. The vessel is open to atmosphere. The bubble generation mechanism is composed of a syringe pump and glass capillary tube (Internal Diameter of 0.45 mm). I connect a 1/4” air line hose from the syringe to the capillary The bubble is formed at the tip...
Thread 'Physics of Stretch: What pressure does a band apply on a cylinder?'
Scenario 1 (figure 1) A continuous loop of elastic material is stretched around two metal bars. The top bar is attached to a load cell that reads force. The lower bar can be moved downwards to stretch the elastic material. The lower bar is moved downwards until the two bars are 1190mm apart, stretching the elastic material. The bars are 5mm thick, so the total internal loop length is 1200mm (1190mm + 5mm + 5mm). At this level of stretch, the load cell reads 45N tensile force. Key numbers...
I'd like to create a thread with links to 3-D Printer resources, including printers and software package suggestions. My motivations are selfish, as I have a 3-D printed project that I'm working on, and I'd like to buy a simple printer and use low cost software to make the first prototype. There are some previous threads about 3-D printing like this: https://www.physicsforums.com/threads/are-3d-printers-easy-to-use-yet.917489/ but none that address the overall topic (unless I've missed...
Back
Top