A few questions about anodization

  • Thread starter Thread starter asdff529
  • Start date Start date
AI Thread Summary
In the anodization of aluminum, the aluminum object acts as the anode while the cathode is typically a carbon rod in a dilute sulfuric acid electrolyte. The process involves applying a voltage (around 12 volts DC) to facilitate the formation of aluminum oxide on the surface, which can penetrate into the metal, creating a durable layer. The discussion highlights a common confusion regarding the discharge order of ions during anodization, specifically why hydroxide ions discharge before aluminum despite aluminum's higher oxidation potential. It is clarified that standard potentials are determined under ideal conditions, but real-world scenarios often involve formal potentials, which can differ significantly and influence the actual discharge order. Additionally, once an aluminum object is anodized, it cannot be anodized again without removing the existing oxide layer, typically through physical means or caustic soda, emphasizing the importance of proper initial anodization for longevity.
asdff529
Messages
38
Reaction score
0
In anodization of aluminium,the aluminium object to be oxidized is the anode,the electrolyte is dilute sulfuric acid the and the aluminium is the cathode
I was taught that the hydroxide ions will preferentially discharge,then the aluminium object will be oxidized by the oxygen formed(?),but i was also taught that according to the electrochemical series,Al should be oxidized first,when does it happen?
Also,if the object is already fully covered by an oxide layer,how can the oxide layer further increase?I mean the inner aluminium part doesn't have and contact with the solution or whatever,how can a reaction occur?
Thank you!
 
Chemistry news on Phys.org
When a voltage of about 12 volts DC of course and a bunch of amps (25 A) is applied to raw aluminum suspended in 15% sulfuric acid bath, with a large carbon rod/pipe/plate as the cathode, anodization occurs. Aluminum oxide forms at the surface and continues down into the metal, forming crystalline aluminum oxide around pores that contain the sulfuric acid, and continue to conduct electricity to the metal. These can grow down into the metal for quite a way, until the hard layer is quite think (in microns).
When the aluminum is removed and washed, you can't anodize it again without stripping off the existing oxide coat, usually physically or with caustic soda (NaOH). This is messy. Do it right the first time and your aluminum anodized coat will last indefinitely.
 
  • Like
Likes 1 person
but how about the priority of discharging.i mean why hydroxide ions is discharged first,instead of Al
Thank you!
 
Are you deciding on the order of the oxidation by comparing standard potentials?
 
Borek said:
Are you deciding on the order of the oxidation by comparing standard potentials?

um...i think so because i haven't been taught about the standard potential.i was just told to memorize the order of the oxidation,without understanding it.
 
I am afraid that's not enough. Standard potentials reflect what is happening in standard conditions, that is, when activities of all involved substances equal 1. In the real solution we deal with so called formal potentials - they can be calculated from the Nernst equation (with standard potential being just a starting point), and they are often substantially different from the standard ones, to the point when the order of oxidation/reduction is reversed.
 
  • Like
Likes 1 person
I want to test a humidity sensor with one or more saturated salt solutions. The table salt that I have on hand contains one of two anticaking agents, calcium silicate or sodium aluminosilicate. Will the presence of either of these additives (or iodine for that matter) significantly affect the equilibrium humidity? I searched and all the how-to-do-it guides did not address this question. One research paper I found reported that at 1.5% w/w calcium silicate increased the deliquescent point by...
I was introduced to the Octet Rule recently and make me wonder, why does 8 valence electrons or a full p orbital always make an element inert? What is so special with a full p orbital? Like take Calcium for an example, its outer orbital is filled but its only the s orbital thats filled so its still reactive not so much as the Alkaline metals but still pretty reactive. Can someone explain it to me? Thanks!!
I'm trying to find a cheap DIY method to etch holes of various shapes through 0.3mm Aluminium sheet using 5-10% Sodium Hydroxide. The idea is to apply a resist to the Aluminium then selectively ablate it off using a diode laser cutter and then dissolve away the Aluminium using Sodium Hydroxide. By cheap I mean resists costing say £20 in small quantities. The Internet has suggested various resists to try including... Enamel paint (only survived seconds in the NaOH!) Acrylic paint (only...
Back
Top