Calculate Force for Beam Shear Failure

AI Thread Summary
To calculate the force necessary for shear failure in a 1/2" tall tooth made of 303 stainless steel with a cross-sectional area of 0.125", the shear stress equation (Force/Area) can be applied. The failure was attributed to repetitive stress rather than a blunt force, with the component operating at approximately -5C. The fracture surface exhibited both crystalline and dull characteristics, indicating a mix of brittle and ductile failure modes. It is important to note that gear tooth forces are complex, and stress concentrations can significantly affect the results. A coarse failure load can be estimated by multiplying the shear strength of the material by the area, but this will only provide an upper bound for the actual forces involved.
Hockeyguy2026
Messages
3
Reaction score
0
I started a new job two weeks ago and I've been out of school for twenty years and have not used strength of materials knowlegde since. I had a part fail in the lab and I would like to calculate the force that would have been necessary to cause the shear failure. I have simplified the problem to a 1/2" tall tooth with a cross section area of .125". The material is 303 stainless steel. Can anyone help me with the equation to find this force. I understand that the part failure was caused by repeative stress and not a blunt force but my first step is to find that blunt force value.
 
Engineering news on Phys.org
What temperature was the component running at at failure?
 
The temperature was below freezing - approx. -5C. The failed compent was from an ice maker.
 
OK so standard quoted materials properties would apply.

Shear stress = Force/area

So you can calculate a coarse failure load by multiplying the shear stength of your steel by the 1/8 sq inch.

However the forces on gear teeth are much more complex so this will only give you an upper bound. There are significant stress concentrations depending upon the shape of the teeth.

Also, what did the fracture surface look like? Can you describe it?
Was it crystalline and shiny or dull and smooth? or was it part crystalline and part dull?
 
The failure looks part crystalline and part dull. The part that broke off is a stream divider that changes the flow of ice from an evaporator to a nozzle that pushes the ice through a tube. The part failed after many months of 24/7 operation.
 
The crystalline part is brittle failure, the dull part ductile failure.
 
Thread 'Physics of Stretch: What pressure does a band apply on a cylinder?'
Scenario 1 (figure 1) A continuous loop of elastic material is stretched around two metal bars. The top bar is attached to a load cell that reads force. The lower bar can be moved downwards to stretch the elastic material. The lower bar is moved downwards until the two bars are 1190mm apart, stretching the elastic material. The bars are 5mm thick, so the total internal loop length is 1200mm (1190mm + 5mm + 5mm). At this level of stretch, the load cell reads 45N tensile force. Key numbers...
I'm trying to decide what size and type of galvanized steel I need for 2 cantilever extensions. The cantilever is 5 ft. The space between the two cantilever arms is a 17 ft Gap the center 7 ft of the 17 ft Gap we'll need to Bear approximately 17,000 lb spread evenly from the front of the cantilever to the back of the cantilever over 5 ft. I will put support beams across these cantilever arms to support the load evenly
Back
Top