How is austenitic stainless steel made?

AI Thread Summary
Austenitic stainless steel is primarily produced by adding high chromium and around 10% nickel, which prevents the transformation to other phases like cementite and ferrite during cooling. The cooling process is crucial, as quenching leads to martensite formation, while austenitic stainless steel is often kept in a solution-annealed condition to maintain its structure. Nickel is essential in inhibiting transformations, while ferritic stainless steels typically contain only chromium. The discussion also touches on the effects of alloying elements on steel properties and the impact of processing methods like forging or working on strength. Understanding these factors is vital for applications requiring specific material characteristics.
Ask1122
Messages
51
Reaction score
0
Hi all, just wanted to find out how is austenitic stainless steel made? Because when you heat the steel above certain temperature, your cementite starts to diffuse out and austenite starts to form, but the thing is this: if you allow the austenite to cool down, it reverts back to cementite and ferrite, and if you quench it you will get martensite, but then how do you cool down the austenitic stainless steel to keep the austenite?

Thanks!
 
Engineering news on Phys.org
A variety of alloying components inhibit the transformation from austenite to other phases. A typical 300 series stainless will have high chromium content and usually ~10% nickel, which prevents the transformation. Other additives are often used to reduce nickel content, keeping costs down.
 
Thx Timmay, that make much more sense to me now. But then does it mean that all austenitic stainless steel comes in a solution annealed condition, I saw somewhere that austenitic stainless steel are not normalised, but i am not sure why?

And if the nickel and chromium prevent the transformation of austenitic stainless steel into pearlites, then how are ferritic stainless steel (e.g. gr 430) made? I see that there are only chromium in the martensitic and ferritic stainless steel, does it mean that Nickel is the only elements that prevents the transformation?

And my last question is if you by any chance know where the creep temperature range for the materials are in ASME?

Thank you for all your help!
 
These articles might be of interest:

Alloy steels
Index - http://steel.keytometals.com/default.aspx?ID=Articles#p5
Alloy steels - http://steel.keytometals.com/default.aspx?ID=CheckArticle&NM=4

Characteristic of alloying elements
http://steel.keytometals.com/default.aspx?ID=CheckArticle&NM=10

Effects on the martensite, pearlite and bainite formation
http://steel.keytometals.com/default.aspx?ID=CheckArticle&NM=51


Steels and their properties are often given in the annealed condition, but they can be forged or hot/cold worked, which does effect strength.
 
Last edited by a moderator: