Keel design, high tensile steel elongation

AI Thread Summary
The discussion centers on the evaluation of a keel design made from high tensile (HT) steel, specifically addressing its deflection and elongation under load. The keel, measuring 1.64m with a 445kg bulb, experiences a deflection of 17mm, raising concerns about whether this indicates failure due to exceeding the 0.2% elongation threshold. It is clarified that the bending stress calculated is approximately 78 MPa, which does not exceed the material's yield strength, suggesting the keel is not overstressed. The elongation for mild steel is calculated to be 0.04%, significantly below the yield strain, confirming that the design is safe. Overall, the keel design appears structurally sound based on the provided calculations.
idfka909
Messages
3
Reaction score
0
To simplify things, I have assumed the keel section is a rectangle and not a foil.

(Also, these specs are taken from an existing design.)

dimensions:

keel 38cm (width/chord) X 3.8cm (height/thick), length 1.64m,

bulb 445Kg Using beamboy, (cantilever with weight at end) the deflection is:-

Using a mass of 445Kg, Moment of Inertia of 380mmX38mm = 1740000, Gpa 210, distance to mid 19mm

Gives a deflection of 17mm.What I would like to know, is this considered a failure. ie the steel was stressed more the 0.2% allowed.
About this allowed 0.2% elongation:-

From a rod rigging spec, 1mm^2 can support 140Kg. = 0.7% elongation. So how does HT steel develop its strength. All steel has approx. the same Modulus of Elasticity, but different ultimate strength, then does it mean that HT steel is allowed to elongate more, ie to 0.7%?

But the yield of point of HT is not well defined, so 0.2% is used?

I'm a little muddled.

thanks,
 
Engineering news on Phys.org
For different steels, the key parameter used in stress analysis is the yield stress. This stress value represents the upper limit of elastic behavior in the material. Elastic behavior in this context means that when the material is loaded, a certain strain is created. Once the load is removed, the previous strain disappears, with no permanent set being created.

Typical mild steel (ASTM A-36) has a min. yield of 36000 psi (248 MPa). AISI 4340 steel has a min. yield of about 78000 psi (540 MPa). Both steels have the same Young's modulus (about 209 GPa).

Different HT steels have different yield points, due to alloy composition, heat treatment, etc. If you are going to design using HT steel, you should know which kind you are dealing with.

I can't comment on your keel design calculation because it is not clear what you are trying to analyze.
 
Thanks SteamKing,

Have a cantilevered beam 1.64m long that's deflected 17mm, has it failed? ie. more than 0.2% elongation?

HT steel has a 0.7% allowed elongation?
 
I calculate a bending stress of about 78 MPa (11300 psi) in the keel, assuming the 445 kg bulb is located 1.64 m from the fixed point of the keel. Based on these assumptions, it does not appear that the keel has been overstressed. I am also assuming that the keel is solid steel 38 mm thick.

The .2% elongation is usually referred to when a tensile test is performed on a specially machined bar-shaped test piece. Again, to emphasize my earlier comments, steel design is based on a calculation of stress rather than a measurement of strain. Due to the large number of different steel alloys in use, a proper structural evaluation requires that the particular alloy from which the member is fabricated should be known.
 
idfka909: You can assume you have mild steel (tensile yield strength, Sty = 248 MPa). I think the modulus of elasticity might be as low as E = 200 000 MPa. As mentioned by SteamKing, the bending stress is sigma = 78 MPa. Therefore, if we pretend you have a uniaxial stress state, then your strain (elongation) is epsilon = sigma/E = (78 MPa)/(200 000 MPa) = 0.04 %, which is much less than the yield strain (Sty/E). Therefore, these values indicate the keel is not overstressed nor overstrained. This is not considered a failure. And the cantilever deflection you computed is correct.
 
Last edited:
Many thanks nvn,
 
Thread 'Turbocharging carbureted petrol 2 stroke engines'
Hi everyone, online I ve seen some images about 2 stroke carbureted turbo (motorcycle derivation engine). Now.. In the past in this forum some members spoke about turbocharging 2 stroke but not in sufficient detail. The intake and the exhaust are open at the same time and there are no valves like a 4 stroke. But if you search online you can find carbureted 2stroke turbo sled or the Am6 turbo. The question is: Is really possible turbocharge a 2 stroke carburated(NOT EFI)petrol engine and...
I need some assistance with calculating hp requirements for moving a load. - The 4000lb load is resting on ball bearing rails so friction is effectively zero and will be covered by my added power contingencies. Load: 4000lbs Distance to travel: 10 meters. Time to Travel: 7.5 seconds Need to accelerate the load from a stop to a nominal speed then decelerate coming to a stop. My power delivery method will be a gearmotor driving a gear rack. - I suspect the pinion gear to be about 3-4in in...
Back
Top