Why are UNF threads being used in this high temperature Boiler Code application?

  • Thread starter Thread starter Pkruse
  • Start date Start date
  • Tags Tags
    Bolts
AI Thread Summary
The discussion centers on the use of UNF threads in a high-temperature Boiler Code application, where nickel and chrome alloys are employed. The design engineer approved the use of threaded rods instead of hex bolts due to long lead times and higher costs associated with the latter. He noted that threaded rods are stronger as they eliminate the stress concentrator (KT) between the shank and head of a bolt. While the use of certified fasteners is emphasized for safety and performance, the engineer's choice was influenced by customer preference for UNF threads. Overall, the project utilizes certified materials similar to those found in jet engines, ensuring reliability in the application.
Pkruse
Messages
465
Reaction score
2
I saw the assembly of a high temperature Boiler Code application the other day. They used nickel and Chrome alloys for the high temperatures. I found the flanges to be particularly interesting. They were using UNF threads, which is not common in boilers, and they were using threaded rod with nuts on both ends.

So I talked with the design engineer. He had called out hex bolts on the drawing, but approved the change because they had a long lead time and were much more expensive. He also said that he likes the threaded rods better anyway because they are stronger, because they eliminate a KT between the shank and the head.

He used the UNF threads only because his customer was in love with them.

Have any of you ever considered this KT in one of your designs?
 
Last edited by a moderator:
Engineering news on Phys.org
In critical applications where safety or performance are concerns, it's best practice to use certified fasteners (e.g. fastener lots that have had a statistical sample tested for strength). I could see how an engineer might be interested in the stress concentrator between the shank & head of a bolt if they're designing a bolt from scratch, but in the design of a large system (like a boiler) which uses off-the-shelf fasteners, I doubt you'd take this into account. More likely you'll find certified fasteners which are strong enough for your application.

Using a stud with threads on both ends doesn't strike me as particurally unusual, as long as you're able to find a stud with certified strength equal to that of the equivalent bolt.
 
I'm assuming that all material in this project is certified. They used the same nickel super alloys you see in a jet engine from the same suppliers.
 
How did you find PF?: Via Google search Hi, I have a vessel I 3D printed to investigate single bubble rise. The vessel has a 4 mm gap separated by acrylic panels. This is essentially my viewing chamber where I can record the bubble motion. The vessel is open to atmosphere. The bubble generation mechanism is composed of a syringe pump and glass capillary tube (Internal Diameter of 0.45 mm). I connect a 1/4” air line hose from the syringe to the capillary The bubble is formed at the tip...
Thread 'Calculate minimum RPM to self-balance a CMG on two legs'
Here is a photo of a rough drawing of my apparatus that I have built many times and works. I would like to have a formula to give me the RPM necessary for the gyroscope to balance itself on the two legs (screws). I asked Claude to give me a formula and it gave me the following: Let me calculate the required RPM foreffective stabilization. I'll use the principles of gyroscopicprecession and the moment of inertia. First, let's calculate the keyparameters: 1. Moment of inertia of...
Thread 'Physics of Stretch: What pressure does a band apply on a cylinder?'
Scenario 1 (figure 1) A continuous loop of elastic material is stretched around two metal bars. The top bar is attached to a load cell that reads force. The lower bar can be moved downwards to stretch the elastic material. The lower bar is moved downwards until the two bars are 1190mm apart, stretching the elastic material. The bars are 5mm thick, so the total internal loop length is 1200mm (1190mm + 5mm + 5mm). At this level of stretch, the load cell reads 45N tensile force. Key numbers...