To find the deflection of a 10x10x0.2 cm composite plate after an impact test, additional information is needed, such as the plate's orientation and coordinate system. The plate, made of glass-epoxy with a specific stacking sequence, weighs 24 grams, and the impactor weighs either 24 or 57 grams, impacting at velocities of 0.6 and 1.2 m/s. The strain has been measured in the x-direction, and there is an indication that strain in the y-direction can also be obtained. The test indicates that the plate remains in the elastic region without any damage. Accurate calculations for deflection will require referencing appropriate equations and material properties.