For transporting waste gas at -300°F, finding suitable plastic tubing is challenging, as most materials become brittle at cryogenic temperatures. Polycarbonate is insufficient, while Teflon may work if properly secured to prevent vibration. Metal tubing is generally recommended due to its better temperature tolerance, with specific low-temperature alloys being suitable for this application. Cryogenic delivery hoses are often multilayer metal devices, which enhance safety and durability. Using armored tubing is advised to minimize the risk of catastrophic failure, as plastic can shatter dramatically under these conditions.
imsmooth
Messages
154
Reaction score
13
Maybe someone here will have an idea where I can get some information. I am planning on making liquid nitrogen from air and will need to regenerate waste gas. This gas will be very cold (-300F) and will get transported through some tubing system. Is anyone aware of any plastic tubing material that will tolerate these temperatures? Polycarbonate is the best I have found so far, but it is not good enough.

Otherwise, I will have to use metal tubing.
 
Physics news on Phys.org
I'm thinking teflon tubing might work. Any thoughts?
 
If you need some plasticity, anything that won't turn brittle at these temperatures will be either liquid or extremely soft at room temperatures. Any basic materials you can find to work with will be extremely brittle at -300°F. I would bet on metals being more suitable than plastics, as they tend to have a better range of temperatures. There are some alloys that are designed for low temperatures that aren't prohibitively soft at room temperatures to be worked with.
 
imsmooth said:
Maybe someone here will have an idea where I can get some information. I am planning on making liquid nitrogen from air and will need to regenerate waste gas. This gas will be very cold (-300F) and will get transported through some tubing system. Is anyone aware of any plastic tubing material that will tolerate these temperatures? Polycarbonate is the best I have found so far, but it is not good enough.

Otherwise, I will have to use metal tubing.

Cryogenic delivery hoses are typically multilayer metal devices:

http://www.sigmasystems.com/accessories-tp/hoses/cryo-hoses.htm

The storage vials I use are made of polypropylene, but I think that material would be a poor choice for cryogenic tubing.
 
Last edited by a moderator:
Teflon should be ok. Just make sure you attach it to something so that it can't vibrate (which it will do if you pump LN2 through it) since this will cause it to eventually break. You will NOT be able to bend the tube once it is cold without breaking it, but I hope you've already realized that (If you want a bendable tube you need something metallic).
Also, use an armoured tube if you can find it. It will reduce the chance of the tube exploding. Note my choice of words, when an plastic tube at 77K bursts it does so in quite an spectacular fashion resulting it lots of small bits of plastic (I am speaking from experience here).
Note also that a tube can work really well for years and then suddenly fail, I would not recommend being too close to an uprotected tube (I've had a LN2 shower once when a tube burst, I don't recommend it).
 
Thread 'Gauss' law seems to imply instantaneous electric field'
Imagine a charged sphere at the origin connected through an open switch to a vertical grounded wire. We wish to find an expression for the horizontal component of the electric field at a distance ##\mathbf{r}## from the sphere as it discharges. By using the Lorenz gauge condition: $$\nabla \cdot \mathbf{A} + \frac{1}{c^2}\frac{\partial \phi}{\partial t}=0\tag{1}$$ we find the following retarded solutions to the Maxwell equations If we assume that...
I passed a motorcycle on the highway going the opposite direction. I know I was doing 125/km/h. I estimated that the frequency of his motor dropped by an entire octave, so that's a doubling of the wavelength. My intuition is telling me that's extremely unlikely. I can't actually calculate how fast he was going with just that information, can I? It seems to me, I have to know the absolute frequency of one of those tones, either shifted up or down or unshifted, yes? I tried to mimic the...

Similar threads

Back
Top