- #1
Quentin_alex
- 12
- 0
Hello,
I ran a test on an industrial composite of 30% glass-filled nylon 6, and my melting temperature peak is too low. The range was from -30 C to 275 C. Why could this be happening? Should I suspect the sample pan?
Thanks.
I ran a test on an industrial composite of 30% glass-filled nylon 6, and my melting temperature peak is too low. The range was from -30 C to 275 C. Why could this be happening? Should I suspect the sample pan?
Thanks.